Abstract

We already proposed a W-shaped POF having an index valley of the refractive index at the core-cladding boundary to minimize the modal dispersion in the POFs, and clarified that the additional modal dispersion compensation effect was provided by the W-shaped index profile in wide g range (the index exponent g is the parameter of the index profile). In this paper, to investigate the relationship between the depth of the index valley and bandwidth properties, we fabricated a high NA W-shaped POF and evaluated its bandwidth performance by comparing with those of the conventional GI POP and low NA W-shaped POP. It was experimentally found that the bandwidth of the high NA W-shaped POP was much higher than that of GI POP and low NA W-shaped POP even if the number of p which described the depth of the index valley was small. However, when the index valley was small enough (p < 1.1), the additional modal dispersion compensation effect was not observed.

Original languageEnglish
Title of host publicationPolymer Preprints, Japan
Pages1353
Number of pages1
Volume54
Edition1
Publication statusPublished - 2005
Event54th SPSJ Annual Meeting 2005 - Yokohama, Japan
Duration: 2005 May 252005 May 27

Other

Other54th SPSJ Annual Meeting 2005
CountryJapan
CityYokohama
Period05/5/2505/5/27

Fingerprint

Plastic optical fibers
Dispersion compensation
Bandwidth
Refractive index

Keywords

  • Modal dispersion compensation effect
  • POP
  • W-shaped profile

ASJC Scopus subject areas

  • Engineering(all)

Cite this

Takahashi, K., Ohdoko, K., Nakamura, T., Ishigure, T., & Koike, Y. (2005). Dispersion characteristics of W-shaped polymer optical fiber. In Polymer Preprints, Japan (1 ed., Vol. 54, pp. 1353)

Dispersion characteristics of W-shaped polymer optical fiber. / Takahashi, Keita; Ohdoko, Kunihiro; Nakamura, Takuhiro; Ishigure, Takaaki; Koike, Yasuhiro.

Polymer Preprints, Japan. Vol. 54 1. ed. 2005. p. 1353.

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Takahashi, K, Ohdoko, K, Nakamura, T, Ishigure, T & Koike, Y 2005, Dispersion characteristics of W-shaped polymer optical fiber. in Polymer Preprints, Japan. 1 edn, vol. 54, pp. 1353, 54th SPSJ Annual Meeting 2005, Yokohama, Japan, 05/5/25.
Takahashi K, Ohdoko K, Nakamura T, Ishigure T, Koike Y. Dispersion characteristics of W-shaped polymer optical fiber. In Polymer Preprints, Japan. 1 ed. Vol. 54. 2005. p. 1353
Takahashi, Keita ; Ohdoko, Kunihiro ; Nakamura, Takuhiro ; Ishigure, Takaaki ; Koike, Yasuhiro. / Dispersion characteristics of W-shaped polymer optical fiber. Polymer Preprints, Japan. Vol. 54 1. ed. 2005. pp. 1353
@inproceedings{55388fd7b7d3423eb4c9a72063a0a814,
title = "Dispersion characteristics of W-shaped polymer optical fiber",
abstract = "We already proposed a W-shaped POF having an index valley of the refractive index at the core-cladding boundary to minimize the modal dispersion in the POFs, and clarified that the additional modal dispersion compensation effect was provided by the W-shaped index profile in wide g range (the index exponent g is the parameter of the index profile). In this paper, to investigate the relationship between the depth of the index valley and bandwidth properties, we fabricated a high NA W-shaped POF and evaluated its bandwidth performance by comparing with those of the conventional GI POP and low NA W-shaped POP. It was experimentally found that the bandwidth of the high NA W-shaped POP was much higher than that of GI POP and low NA W-shaped POP even if the number of p which described the depth of the index valley was small. However, when the index valley was small enough (p < 1.1), the additional modal dispersion compensation effect was not observed.",
keywords = "Modal dispersion compensation effect, POP, W-shaped profile",
author = "Keita Takahashi and Kunihiro Ohdoko and Takuhiro Nakamura and Takaaki Ishigure and Yasuhiro Koike",
year = "2005",
language = "English",
volume = "54",
pages = "1353",
booktitle = "Polymer Preprints, Japan",
edition = "1",

}

TY - GEN

T1 - Dispersion characteristics of W-shaped polymer optical fiber

AU - Takahashi, Keita

AU - Ohdoko, Kunihiro

AU - Nakamura, Takuhiro

AU - Ishigure, Takaaki

AU - Koike, Yasuhiro

PY - 2005

Y1 - 2005

N2 - We already proposed a W-shaped POF having an index valley of the refractive index at the core-cladding boundary to minimize the modal dispersion in the POFs, and clarified that the additional modal dispersion compensation effect was provided by the W-shaped index profile in wide g range (the index exponent g is the parameter of the index profile). In this paper, to investigate the relationship between the depth of the index valley and bandwidth properties, we fabricated a high NA W-shaped POF and evaluated its bandwidth performance by comparing with those of the conventional GI POP and low NA W-shaped POP. It was experimentally found that the bandwidth of the high NA W-shaped POP was much higher than that of GI POP and low NA W-shaped POP even if the number of p which described the depth of the index valley was small. However, when the index valley was small enough (p < 1.1), the additional modal dispersion compensation effect was not observed.

AB - We already proposed a W-shaped POF having an index valley of the refractive index at the core-cladding boundary to minimize the modal dispersion in the POFs, and clarified that the additional modal dispersion compensation effect was provided by the W-shaped index profile in wide g range (the index exponent g is the parameter of the index profile). In this paper, to investigate the relationship between the depth of the index valley and bandwidth properties, we fabricated a high NA W-shaped POF and evaluated its bandwidth performance by comparing with those of the conventional GI POP and low NA W-shaped POP. It was experimentally found that the bandwidth of the high NA W-shaped POP was much higher than that of GI POP and low NA W-shaped POP even if the number of p which described the depth of the index valley was small. However, when the index valley was small enough (p < 1.1), the additional modal dispersion compensation effect was not observed.

KW - Modal dispersion compensation effect

KW - POP

KW - W-shaped profile

UR - http://www.scopus.com/inward/record.url?scp=33645649484&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=33645649484&partnerID=8YFLogxK

M3 - Conference contribution

AN - SCOPUS:33645649484

VL - 54

SP - 1353

BT - Polymer Preprints, Japan

ER -