Incipient plasticity in 4H-SiC during quasistatic nanoindentation

Saurav Goel, Jiwang Yan, Xichun Luo, Anupam Agrawal

Research output: Contribution to journalArticlepeer-review

25 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Incipient plasticity in 4H-SiC during quasistatic nanoindentation'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemical Compounds