Abstract

The present work reports the mismatch limit loads for a V-groove welded pipe for a circumferential crack using finite element (FE) analyses. To integrate the effect of groove angles on mismatch limit loads, one geometryrelated slenderness parameter was modified by relevant geometric parameters including the groove angle, crack depth, and root opening based on plastic deformation patterns in the theory of plasticity. Circumferential through-wall cracks are located at the centre of the weldments with two different groove angles (45°, 90°). With regard to the loading conditions, axial (longitudinal) tension and bending are applied for all cases. For the parent and weld metal, elasticperfectly plastic materials are considered to simulate and analyze under- and over-matching conditions in plasticity. The overall results from the proposed solutions are found to be similar to the FE results.

Original languageEnglish
Pages (from-to)1379-1386
Number of pages8
JournalTransactions of the Korean Society of Mechanical Engineers, A
Volume37
Issue number11
DOIs
Publication statusPublished - 2013 Jan 1
Externally publishedYes

Fingerprint

Load limits
Welds
Pipe
Cracks
Defects
Plasticity
Plastic deformation
Plastics
Metals

Keywords

  • Finite element analysis
  • Limit load
  • Strength mismatch
  • V-groove butt weld

ASJC Scopus subject areas

  • Mechanical Engineering

Cite this

Mismatch limit load analyses for V-groove welded pipe with through-wall circumferential defect in centre of weld. / Kim, Sang Hyun; Han, Jae Jun; Chung, Jin Taek; Kim, Yun Jae.

In: Transactions of the Korean Society of Mechanical Engineers, A, Vol. 37, No. 11, 01.01.2013, p. 1379-1386.

Research output: Contribution to journalArticle

@article{11609ee94e454c43b28c0164b90a7131,
title = "Mismatch limit load analyses for V-groove welded pipe with through-wall circumferential defect in centre of weld",
abstract = "The present work reports the mismatch limit loads for a V-groove welded pipe for a circumferential crack using finite element (FE) analyses. To integrate the effect of groove angles on mismatch limit loads, one geometryrelated slenderness parameter was modified by relevant geometric parameters including the groove angle, crack depth, and root opening based on plastic deformation patterns in the theory of plasticity. Circumferential through-wall cracks are located at the centre of the weldments with two different groove angles (45°, 90°). With regard to the loading conditions, axial (longitudinal) tension and bending are applied for all cases. For the parent and weld metal, elasticperfectly plastic materials are considered to simulate and analyze under- and over-matching conditions in plasticity. The overall results from the proposed solutions are found to be similar to the FE results.",
keywords = "Finite element analysis, Limit load, Strength mismatch, V-groove butt weld",
author = "Kim, {Sang Hyun} and Han, {Jae Jun} and Chung, {Jin Taek} and Kim, {Yun Jae}",
year = "2013",
month = "1",
day = "1",
doi = "10.3795/KSME-A.2013.37.11.1379",
language = "English",
volume = "37",
pages = "1379--1386",
journal = "Transactions of the Korean Society of Mechanical Engineers, A",
issn = "1226-4873",
publisher = "Korean Society of Mechanical Engineers",
number = "11",

}

TY - JOUR

T1 - Mismatch limit load analyses for V-groove welded pipe with through-wall circumferential defect in centre of weld

AU - Kim, Sang Hyun

AU - Han, Jae Jun

AU - Chung, Jin Taek

AU - Kim, Yun Jae

PY - 2013/1/1

Y1 - 2013/1/1

N2 - The present work reports the mismatch limit loads for a V-groove welded pipe for a circumferential crack using finite element (FE) analyses. To integrate the effect of groove angles on mismatch limit loads, one geometryrelated slenderness parameter was modified by relevant geometric parameters including the groove angle, crack depth, and root opening based on plastic deformation patterns in the theory of plasticity. Circumferential through-wall cracks are located at the centre of the weldments with two different groove angles (45°, 90°). With regard to the loading conditions, axial (longitudinal) tension and bending are applied for all cases. For the parent and weld metal, elasticperfectly plastic materials are considered to simulate and analyze under- and over-matching conditions in plasticity. The overall results from the proposed solutions are found to be similar to the FE results.

AB - The present work reports the mismatch limit loads for a V-groove welded pipe for a circumferential crack using finite element (FE) analyses. To integrate the effect of groove angles on mismatch limit loads, one geometryrelated slenderness parameter was modified by relevant geometric parameters including the groove angle, crack depth, and root opening based on plastic deformation patterns in the theory of plasticity. Circumferential through-wall cracks are located at the centre of the weldments with two different groove angles (45°, 90°). With regard to the loading conditions, axial (longitudinal) tension and bending are applied for all cases. For the parent and weld metal, elasticperfectly plastic materials are considered to simulate and analyze under- and over-matching conditions in plasticity. The overall results from the proposed solutions are found to be similar to the FE results.

KW - Finite element analysis

KW - Limit load

KW - Strength mismatch

KW - V-groove butt weld

UR - http://www.scopus.com/inward/record.url?scp=84898478882&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84898478882&partnerID=8YFLogxK

U2 - 10.3795/KSME-A.2013.37.11.1379

DO - 10.3795/KSME-A.2013.37.11.1379

M3 - Article

AN - SCOPUS:84898478882

VL - 37

SP - 1379

EP - 1386

JO - Transactions of the Korean Society of Mechanical Engineers, A

JF - Transactions of the Korean Society of Mechanical Engineers, A

SN - 1226-4873

IS - 11

ER -