抄録
The electrochromic transition of a nickel borate thin film between colorless and brown was examined by means of in situ XAFS and UV/vis spectroscopy. The XAFS spectra showed that the average valence state of the nickel species in the film changed from +2.1 to +3.8 following the application of an electrode potential. Additionally, a broad peak at 700nm was observed during in situ UV/vis absorption measurements on the application of a positive potential. These results suggest that the nickel borate film reversibly forms a NiOOH structure with a domain size of several nanometers during the electrochromic reaction.